I'm using a power adapter from an old laptop, outputs 19vdc @ 4.5 amps. The sacrificial metal is iron pipe that I cut into sections, and the solution is water and washing soda. Workpiece is ground, and the sacrificial metal (anode) is positive. Last edited on Mon Aug 27th, 2018 09:00 pm by jsoluna |
||||||||
|